Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

A105N versus SA105N

Status
Not open for further replies.

Sabrean

Mechanical
Sep 5, 2007
2
Hi everyone,

Do any of you know if there is a difference between A105N and SA105N carbon steels ?

Thanks
 
Replies continue below

Recommended for you

A 105N material is supplied under an ASTM specification, while SA 105N material is supplied under an ASME specification. There are no differences between these two specifications (ASME SA 105-98).
 
ASME SA 105 (in the 2007 ASME Section IIA) is identical to ASTM A 105-2003. The current version of ASTM A105 is 2005. The only change that has occurred since the 2003 version is:

Revised 12.2.2 to require reporting the width of the gage length of longitudinal strip tensile specimens, if they are used.

If this change does not affect you, then the two are the same. The ASME version usually lags the ASTM version.
 