For pipe Flange, our inquiry has been A350LF2. Vendor suggested A105N/A350LF2. Can you help me what is this dual material? Does it cover requirement for A350LF2?
 
It is not a dual material, but dual certified. The material conforms to both the specs.

Since your enquiry was for A350LF2, you need to check whether the MTCs / MTRs conform to ASTM A 350 Gr LF2 only.

DHURJATI SEN


 
Thank you very much @DHURJATI
 
I have seen material supplied to 4 or 5 different specs at once. As long as it fully meets the requirements for the one that you are concerned with then you are fine.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 