The A- no is a designation used by ASME B&PV (Boiler and Pressure Vessel) Code, Section IX that relates to a common chemical composition for weld filler metal. Get a copy of Section IX and review it. Section IX is one of 12 book sections that deals with welding procedure and welder qualification along with brazing.