What do the dashes mean in QW-442? Can additions of Ni, Mo, and Cr be added to A No. 1 filler metal and still meet this classification if it does not meet other classifications?
 
The dots mean not specified. Look at SA 751 for understanding nomenclature related to chemical analysis.
 