We are using K0006 in bar form from 30Diameter up to 130 diameter.
I would like to cold forge K0006 35mm Diameter and 50mm long as well as 40mm diameter and 50mm long
we receive the steel form Macsteel full annealed and we then Spheroidize the steel.
at present we CNC turn the drill bits but there is better strength in forging as well as taper control.
i would like to cold forge the hole bit inside taper and out side design and then mill the relief on the out side afterwords
do you Know any company that can forge this properly and are there any new advancements in steel in this application for impact and wear as well as holding a 3 micro interference fit of carbide buttons on the head.
i am also looking for a reliable Heat treatment company that can HT and austemper the bits with in spec ( my biggest problem is body failure dew to HT not correct).
Regards Alan