Hello everyone
I need guidance in choosing a welding material for welding
Half pipe jacket reactor .
The reactor made of 904-L and the half pipe jacket made of 304-L(Contains steam at 160 °c)
What is the recommended welding material 904-L or 304-L
Thanks
Aloni
 
Replies continue below

Recommended for you

What did your welding supplier suggest?
Have you looked to see what Miller or Lincoln have in their books?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Hi
Avesta 904-l (E385-17)
Or avesta p5 (E309MoL-17)

Rrgards
Alon
 
As others have said welding 904L to itself can be problematic.
I would look into using the 309MO or a 310MO first.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 