I need some help in regards to 800HT piping. Last year my company welded several joints in 800HT piping using Inco82 filler 14” SCH..312. Now about ½” from the weld toe in the HAZ the plant is experiencing t/w cracking. The system runs over 1000°f during service. My question is our PQR and WPS for P45 list no PWHT. I am aware of the requirements noted in SEC VIII Div. III for PWHT of 800HT however the code of construction for this job was B31.1 and B31.3. Are we wrong for not PWHT the joints?