Jan 8, 2013 #1 kevlar49 Materials Joined Jun 1, 2006 Messages 287 Location US Aluminum heat treated to T651 will impart better dimensional stability than T6. Can the same be said for T7352 vs T73?
Aluminum heat treated to T651 will impart better dimensional stability than T6. Can the same be said for T7352 vs T73?
Jan 8, 2013 #2 swall Materials Joined Sep 30, 2003 Messages 2,767 Location US Your question can not be answered unless you get more specific about product form and intended application. Upvote 0 Downvote
Your question can not be answered unless you get more specific about product form and intended application.
Jan 8, 2013 Thread starter #3 kevlar49 Materials Joined Jun 1, 2006 Messages 287 Location US forging per AMS 4147 or 4141. Machined flange. Upvote 0 Downvote
Jan 9, 2013 1 #4 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US In general, the T7352 will have better dimensional stability. Upvote 0 Downvote