Aluminum heat treated to T651 will impart better dimensional stability than T6. Can the same be said for T7352 vs T73?
 
Your question can not be answered unless you get more specific about product form and intended application.
 
forging per AMS 4147 or 4141. Machined flange.
 
In general, the T7352 will have better dimensional stability.
 