Does anyone have a reference I can access that will show the microstructure for 7050 aluminum (T7452 heat treated condition)? I have an impeller reportedly machined from a forged 'billet' and would like to compare the microstructure I have with what is typical for this condition.
Screenshot 2025-05-12 155556.png
 
Replies continue below

Recommended for you

OP
There should be examples in the ASM heat treating hand book. Don't remember the upto date volume.
 
OP
Also AMS material specification for this material for castings and wrought material.
 