Nov 7, 2003 #1 taskusa Mechanical Joined Nov 7, 2003 Messages 2 Location US Im looking at a job for a pool house and the eupitiment inside is mande with 6063 alum tubing. I wonderering if there is going to be a corrision issue with the chlorine?
Im looking at a job for a pool house and the eupitiment inside is mande with 6063 alum tubing. I wonderering if there is going to be a corrision issue with the chlorine?
Nov 7, 2003 #2 kenvlach Materials Joined Apr 12, 2000 Messages 2,514 Location US Yes, you would get the following: 2 Al + 3 Cl2 = 2 AlCl3 Suggest having the aluminum chromated and powder coated. Upvote 0 Downvote
Yes, you would get the following: 2 Al + 3 Cl2 = 2 AlCl3 Suggest having the aluminum chromated and powder coated.