Would some really good metallurgist go up to thread108-326877
and see if there is a metallurgical reason for what the OP has posted regarding Eaton's claim that grease degrades 5160 spring steel? Even if you aren't a good metallurgist, give it a try anyway.

rmw
 
Replies continue below

Recommended for you

Maui replied to the thread in question, as did I. We are both metallurgists.
 