I am working on a project that will require large volumes of 5120H steel round bar. I have been able to get prices for mill run material however we are moving into the prototype stage right now and I cannot find a source for small volume. Does anyone know of a supplier that would have this material for prototype quantities?
 
Replies continue below

Recommended for you

5120H material spec? ASTM, AISI, AMS... etc.

Also any special features, such as 'as received HT', required HT for service, allowed decarburization, min toughness @ HT, min/max stock dimensions, etc...

Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion"]
o Learn the rules like a pro, so you can b
 
Good luck finding that, we always have to use 8620 for initial prototype work until we get the full mill order for 5120.
 
I received a reply to a query for small qauntity from the following:

fiona@bscglobe.com <fiona@bscglobe.com>

Thanks for your interesting in our products. This is Fiona from BSC group.

We got your inquiry about our product ASE5120H ,and before we send you the offer please clarify below information to complete the quotation:

1. What kind of machine you are plan to manufacture ?

2. Do you need sheet ? pipe or ? may i have the confirmed size as well ?

3. What will be your quantity ?