can anyone help me out with cutting conditions for .500 steel im having a hard time getting a clean cut????????
Thank yall[afro]
 
evans I think ur in MM so 40 in ur measurement would be 1016 I think I would double check that but u can probably compare and confirm [morning]
 
if your feed rate is .40, wouldn't that be meters per min?

Evans - 25.4 mm = 1 inch
 
-LaserSpyder - after digging into my laser a little bit more i realized there was a larger problem then my cut conditions. My A/O mirror was not adjusting when it needed too. Now we are currently replacing the Air pressure regulator for the A/O.

On a side note - how fast are you able to cut 1/4" like butter?

 
FabProHelp that should make a huge difference in cut, and my cut conditions for .250 steel are ....
FR 90. PWR 3600 FREQ 1000 Duty 90% GAS P. 0.07 GAS TIme 0.5 GAP .040........how does ur .250 cut?
 
Before we replaced the Air pressure regulator, my 1/4" was cutting amazing but I had my feed rate down to 60 in/min. Just started to re-adjust the settings now and they cut clean at 78 in/min. I am going to try ramping them up to your settings and see if I can get closer to 90 in/min.

I will keep you updated.... hopefully this corrects my 1/2" cutting issue
 
LaserSpyder - How deep do you have to drive your focus to cut that quickly?
 
my focus (focal(inch)) is set to -0.031 sorry I meant to put that in but didn't [laser]
 
FabProHelp we recently replace our (NC programmable assist gas regulator" p/n 71359715 NC regulator) ......... and OH MAN did our cuts IMPROVE! our 190Alum is cutting better then ever and that was our #1 problematic material and thickness, and we never even suspected there was anything wrong with our assist gasses.[machinegun]

 
What do you consider to be the max thickness you cut on your FO3015? Steel - Aluminum - Stainless Steel
 
I don't cut steel but aluminum I can cut .375 and stainless I cut 1.000" with my fo3015 4kw resonator
 
20171002_140630_llyqdz.jpg
20171002_140630_luazva.jpg
here's some pics of 1" stainless on my 4kw
 
now I want to cut some 1" [deejay] ..... I bet u can clean those cuts up a bit with your gas pressure and driving focus down a little deeper I think anywho [machinegun]
 
The pierce is the hard part and I only get 17 bar out of my machine.
 
I'm looking for some inner cut conditions for 3/4" carbon steel. I can cut the perimeter great, can't cut holes .500". Terrible.
My focus is at .142. I see posts where the focus numbers are low.
 
Laser Lozer can u post a pic of ur cut conditions?
 