Did you test 440C with a higher anneal temp? You can match the lower properties.
What strength level do you use the 440A? Do you know what temper temp and hardness you are using?
There are other martensitic alloys out there.
If you want similar strength and corrosion resistance I would start with 425mod, 455, 420F, or 431.
Good luck.
= = = = = = = = = = = = = = = = = = = =