Does anyone know if type 415 stainless plate is available anywhere. (this is the wrought version of CA6NM castings) I don't know of anyone that can supply this material so far.
 
I went through a Reliance and a Ryerson catalog - only 410, 410S, and 430 plate available there. Saw 416 in rounds and squares. What application would you use 415 for? [atom]
 
Don't know the specific application, but we would be welding it to a CA6NM casting, and our engineer wants it to have the same chem/mech properties, so I know I could get a forge shop to make F6NM bars, but I though it would be cheaper to get a plate cut if I can find one.
 
That's too rare a grade to find in plate. You would have to order a heat lot ( 100 tons ). Advise your engineer to think a little more practically.
 
A suggestion would be to use 15-5PH or 17-4PH stainless plate. It's generally available, and is fairly close to the CA6NM metallurgy. Should be cheaper than 304SS too.
 