We have a company mats spec that requires forged bar that we buy in to have been normalised before Q+T.
In my structural steel experience, normalising has been pretty much superceded these days. Eg in Rolled structural steels, controlled rolling is used where lower temps in the last stages of hot rolling are employed to control austenite grain size so that it transforms to a fine grained ferrite.
So do they do they same thing in forged bar?
We have been offered some 6inch 80ksi 4140mod but the supplier has noted that it does not meet our mat spec to be normalized prior to Q+T.
In my structural steel experience, normalising has been pretty much superceded these days. Eg in Rolled structural steels, controlled rolling is used where lower temps in the last stages of hot rolling are employed to control austenite grain size so that it transforms to a fine grained ferrite.
So do they do they same thing in forged bar?
We have been offered some 6inch 80ksi 4140mod but the supplier has noted that it does not meet our mat spec to be normalized prior to Q+T.