The AWS D 1.1 shows no grouping for this steel, what sort of rods can be used and where can I find guidance on similar non grouped materials for the AWS and ASME.
 
Check out this thread: thread725-69145
If it is not listed in the D1.1, Table 3.1, then procedure qualification is in order.
 
What are other the major variables in rod selection with materials, I know strength and position , but what are the others?
 