Sep 3, 2003 #1 IAL2002 Mechanical Joined Jul 23, 2003 Messages 9 Location TT The AWS D 1.1 shows no grouping for this steel, what sort of rods can be used and where can I find guidance on similar non grouped materials for the AWS and ASME.
The AWS D 1.1 shows no grouping for this steel, what sort of rods can be used and where can I find guidance on similar non grouped materials for the AWS and ASME.
Sep 3, 2003 #2 CWIC Specifier/Regulator Joined Feb 14, 2003 Messages 245 Location US Check out this thread: thread725-69145 If it is not listed in the D1.1, Table 3.1, then procedure qualification is in order. Upvote 0 Downvote
Check out this thread: thread725-69145 If it is not listed in the D1.1, Table 3.1, then procedure qualification is in order.
Sep 4, 2003 Thread starter #3 IAL2002 Mechanical Joined Jul 23, 2003 Messages 9 Location TT What are other the major variables in rod selection with materials, I know strength and position , but what are the others? Upvote 0 Downvote
What are other the major variables in rod selection with materials, I know strength and position , but what are the others?