Well in this thread {thread330-123117} I described a problem encountered in the production of a set of prototypes. Teh customer was informed of the problem with carburization. Engineering data was exchanged and the print was updated as far as the material call out.
Just to re-hash:
4130
50mmX15mmx6mm
is 45-49HRc too high of a spec for Q&T of this size of part? I would like an oil quench to reduce the severity, however normally all we do is supply the material type and the final required hardness.
thanks.
(yes I've checked the TTT curves this time.
Just to re-hash:
4130
50mmX15mmx6mm
is 45-49HRc too high of a spec for Q&T of this size of part? I would like an oil quench to reduce the severity, however normally all we do is supply the material type and the final required hardness.
thanks.
(yes I've checked the TTT curves this time.