I am attemping to allieviate erosion in several control valves by sleeving the body with a hardened alloy. I have settled on 4130 as it is all that is available short of boring solid round stock. I am considering flame hardening these sleeves to obtain maximum hardness. Wall thickness is .125, 3" O.D. I think that raising the temp to 1600 and then water quench will give me a hardness of at least 35 Rc. Can anyone comment on this. Will I be able to weld the sleeves to the 316L body after hardening, Will the diameter of the sleeve be greater due to Martensite presence, any guesses on shrinkage or growth?
Thanks