twistedneck
Automotive
Hi this is my first post here!
I'm planning to Austemper a rectangular structure of 4130 sheet steel, 1mm thick, appox 10" long, 1.5" box. I'm creating some small stampings and dimples on this structure as well, so there will be a lot of stresses built up.
Goals are to obtain toughness, hardness and reduce warping. I plant to normalize first, then fix any warping, then Austenetize.
I'm shooting for Austemper in Nitric / Nitrite salt at 720F (MS = 710F). Goal is 45 RC.
Austenetize in a foil envelope at 1600F..
How long do i hold 4130 at 720F? I can't find a good 4130 TTT.
Is there any way i can dip the temp to 710F (MS Temp) and retain the lower bainite toughess?
Please comment isothermal transformations and reduced warping. Thanks.
I'm planning to Austemper a rectangular structure of 4130 sheet steel, 1mm thick, appox 10" long, 1.5" box. I'm creating some small stampings and dimples on this structure as well, so there will be a lot of stresses built up.
Goals are to obtain toughness, hardness and reduce warping. I plant to normalize first, then fix any warping, then Austenetize.
I'm shooting for Austemper in Nitric / Nitrite salt at 720F (MS = 710F). Goal is 45 RC.
Austenetize in a foil envelope at 1600F..
How long do i hold 4130 at 720F? I can't find a good 4130 TTT.
Is there any way i can dip the temp to 710F (MS Temp) and retain the lower bainite toughess?
Please comment isothermal transformations and reduced warping. Thanks.