May 19, 2009 #1 antoine66 Materials Joined Jun 2, 2008 Messages 6 Location FR Hi All, What is the most commonly used standard for corrosion resistance testing of stainless type 410 S? We are performing welding and heat treatments and would like to ensure corrosion resistance is not hampered.
Hi All, What is the most commonly used standard for corrosion resistance testing of stainless type 410 S? We are performing welding and heat treatments and would like to ensure corrosion resistance is not hampered.
May 19, 2009 #2 cloa Petroleum Joined Jul 18, 2008 Messages 1,071 Location JP In what environment? Upvote 0 Downvote
May 19, 2009 1 #3 gr2vessels Mechanical Joined Sep 29, 2004 Messages 1,971 Location AU Refer to ASTM G157, Outokumpu MTI-1 procedure;- use the documents referenced in these standards for further info. Cheers, gr2vessels Upvote 0 Downvote
Refer to ASTM G157, Outokumpu MTI-1 procedure;- use the documents referenced in these standards for further info. Cheers, gr2vessels
May 19, 2009 Thread starter #4 antoine66 Materials Joined Jun 2, 2008 Messages 6 Location FR Cloa, We are suplying 410S clad plates for coke drums application in refineries. Upvote 0 Downvote
May 19, 2009 Thread starter #5 antoine66 Materials Joined Jun 2, 2008 Messages 6 Location FR Thanks gr2vessels for this interesting reference. Upvote 0 Downvote