123Cat
Mechanical
- Jul 16, 2003
- 67
I have wire cut a 40 mm 12 tooth , 0.5 mm lamination thickness stator piece , there are 16 pieces
Im doing a skip tooth Classic LRK wind
large prop at about 4000 RPM
Do I need to anneal the stator pieces after wire cutting
Does wire cutting greatly effect the properties of the steel or does it not ,
Thank you very much
By the way it is 0.5mm thick electrical steel from an old transformer
Im doing a skip tooth Classic LRK wind
large prop at about 4000 RPM
Do I need to anneal the stator pieces after wire cutting
Does wire cutting greatly effect the properties of the steel or does it not ,
Thank you very much
By the way it is 0.5mm thick electrical steel from an old transformer