I have wire cut a 40 mm 12 tooth , 0.5 mm lamination thickness stator piece , there are 16 pieces

Im doing a skip tooth Classic LRK wind

large prop at about 4000 RPM

Do I need to anneal the stator pieces after wire cutting

Does wire cutting greatly effect the properties of the steel or does it not ,

Thank you very much

By the way it is 0.5mm thick electrical steel from an old transformer
 