A vendor for us is wanting to use this material for a small oil pump shaft. The shaft has very low torsion so that is not much of a concern at all. However, we specify a surface hardness of HRC58-65 due to an oil seal that rides on the shaft. These were previously done by carborizing 8620. We are trying to keep costs down and vendor is recommending this material at I assume it's full hardness of HRC58.
Shaft is also subject to constant vibration so if all the toughness is gone, vibration could be an issue. The diam of shaft is 3/8" but end with pump gear is only 1/4" threaded.