Hi

I am looking for 3D orthotropic or 3D Anisotropic properties for the honeycomb core F40 3.1 pcf Flexcore (5052 AL)

Does anyone have these properties?

It will be of much helpful.

Thanks
 
There is an SAE AMS spec for this core. Don't recall number. It will have thru thickness shear and normal modulus. Use low, near zero values for the Inplane values.
 