TCGT

Mechanical
Oct 26, 2007
43
I have an Italian print that calls out a material of 39NiCrMo3. Do you know what an equivalent US steel would be for this material? I have seen on the web that some manufacturers will say that AISI9840 is the same but it seems as if this steel isn't commonly used in the US.

The part is a gib that is used on a spindle mounting.

Any help you can provide would be appreciated.
 
Replies continue below

Recommended for you

If you are looking for a commonly available material, the you should use 4340. It is not an equivalent, but it is a suitable alternative.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 