I have an oilfield application with 316SS & 17-4Ph H1150D components. Our customer has cited corrosion & pitting problems with 316SS in the high temp (300F - 500F) salt spray environment and requires a material change.
The 316SS components are 1" AutoClave Medium Pressure (20K) fittings (coned & threaded nipple, gland nut, collar) and a 1/4" medium pressure angle valve with nipples, gland nuts, and collars. These components are connected to the 17-4Ph body.
We are looking at changing the 1" & 1/4" nipples to either 725, 2205, or 2507. Based on the AutoClave Material vs Pressure & Pressure vs Temperature charts HC-276 is the closest replacement for the fitting parts & the 1/4" angle valve.
Does anyone have any other material recommendations?
Should I be concerned about gall potential between any of the components/materials I mentioned?
Thanks for your assistance.
Louis
The 316SS components are 1" AutoClave Medium Pressure (20K) fittings (coned & threaded nipple, gland nut, collar) and a 1/4" medium pressure angle valve with nipples, gland nuts, and collars. These components are connected to the 17-4Ph body.
We are looking at changing the 1" & 1/4" nipples to either 725, 2205, or 2507. Based on the AutoClave Material vs Pressure & Pressure vs Temperature charts HC-276 is the closest replacement for the fitting parts & the 1/4" angle valve.
Does anyone have any other material recommendations?
Should I be concerned about gall potential between any of the components/materials I mentioned?
Thanks for your assistance.