Hi,
I have two parts, one made from 316 SS and one made from 17-4 SS. They were both exposed to the same substance, I don't know what this substance was but it corroded the 17-4 until it fell apart and left the 316 SS in mint condition. Does anyone have any thoughts on what kind of of substance or chemical could cause a complete break down of 17-4 and leave 316 unaffected?
Thanks all.
I have two parts, one made from 316 SS and one made from 17-4 SS. They were both exposed to the same substance, I don't know what this substance was but it corroded the 17-4 until it fell apart and left the 316 SS in mint condition. Does anyone have any thoughts on what kind of of substance or chemical could cause a complete break down of 17-4 and leave 316 unaffected?