Do you know of a website that lists properties of various stainless steels?

I am specifically looking for the allowable bending stress and allowable shear stress of 316 SS.

Is there ever an occassion where people design to the ultimate tensile strength limit as opposed to the yield strength?

Do the stress values presented in textbooks generally include a safety factor? I assume not, but wanted to get input from others!!!

Thanks for your assistance,
Charlie
 
I believe the ultimate tensile for 316SS is 58 ksi and the shear stress is 60% of this amount. The yield for 316 SS is 30ksi. I do not know a good website for this. I would love to find one...
 
There does not seem to be a definitive answer for every situation. See the responses from the folks in the "Stainless Steel For Engineers" Forum, at thread723-152250

[idea]
 
The ultimate and yield strengths of stainless steels (including 316) vary depending on the alloy and the finishing conditions, whether cold worked or annealed. If it is cold worked, it has a much higher strength. You'll need to know these things before you start designing to any limits.

For material properties go to
 
I think the allowables will depend on the application as well- seems like values for flanges are lower than for plate, for example.
 