Does anyone know where to get data on 304SS fatigue limit? The number of load cycles the material can take at a certain stress? My college text book Mechanics of Materials by E.P. Popov has a graph for 18-8 which is a generic term for 304 but does not say if the specimens were annealed or drawn or hot/cold rolled or what. It also has the curve flattening out toward infinite life at about 95,000psi which is way higher than I expected. This is above the tensile strength for commercial plate. The unguaranteed value for tensile in my steel catalog was only 75,000psi. It does not seem logical for materials capability to increase with cyclic loading. Can anyone help me?