Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

304 Vs 316 Stainless steel 1

Status
Not open for further replies.

johnddd

Industrial
Joined
Jul 23, 2019
Messages
1
Location
IN
What is difference between 304 Vs 316 Stainless steel?
 
The answer is on Google. This is too ‘easy’ for us to expand on. Do a search on this site and you’ll find similar threads have covered this topic.
Come back if you have any specific questions

Huub
- You never get what you expect, you only get what you inspect.
 
What are you doing? Why do you care?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
12

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
SnT, I see the answer as 4, (2 Ni and 2 Mo).

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Well, yeah, you're the metallurgist :)

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
From the operators perspective the difference is about 30. That's 30% more expensive.
 
When bright annealed in very dry hydrogen 304 is yellower and 316 is bluer, if your eyes are good enough (and lighting is good also) to see it.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Next to nothing, when comparing corrosion resistance...
 
316 is marginally better, I agree. The additional Mo helps mostly against pitting corrosion. But neither is worth much in a susceptible, chloride-rich environment.
 
The only real difference in Cl pitting resistance is the time to initiation, not the inevitability of corrosion.

= = = = = = = = = = = = = = = = = = = =