3 wire truss mesh availability?

Status
Not open for further replies.
H&B says they discontinued their 130 (3-wire) Truss Mesh for a 14" wide wall ... WIRE_BOND says they can provide it, but is special order and a three week lead time. is there any other company out there that has it readily available?
 
 3 wire Truss Mesh
The industry is moving away from truss type reinforcement since it may interfere with vertical rebar. Ladder type joint reinforcement provides the same strength as truss type - its the side wires which do all the work, not the cross wires. So unless you have a special condition use ladder type joint reinforcement.
 