Hi All,
Does anyone have a spec on the designed torque load specs for 3/8-16, Hex, 3 projection, weld nuts?
I have a client that has rejected my parts due to the weld nuts failing under torque.
We used the Nut MFGs weld specs & did an informal load test. Which seemed to be sufficient, for several orders.
Neither the customer nor the MFG had a statement of how to test or what load was spec'd.
Now we've had several failures, per the client.
So, I'm looking for some form of statement to use as a guide for my customer & I to agree on, for setting the
torque load requirement.
Any help is always appreciated.
Thanks in advance.
Does anyone have a spec on the designed torque load specs for 3/8-16, Hex, 3 projection, weld nuts?
I have a client that has rejected my parts due to the weld nuts failing under torque.
We used the Nut MFGs weld specs & did an informal load test. Which seemed to be sufficient, for several orders.
Neither the customer nor the MFG had a statement of how to test or what load was spec'd.
Now we've had several failures, per the client.
So, I'm looking for some form of statement to use as a guide for my customer & I to agree on, for setting the
torque load requirement.
Any help is always appreciated.
Thanks in advance.