Johnson 123
BE CAUTIOUS: bearing [crushing] strength of a washer is an important mechanical feature. IF understrength [low yield/crush], then joint will likely loosen in-service!
Per MIL-HDBK-698, Table XXI...
Alloy 360 [KSI]...
Strain temper UTS TYS %El
H [<0.187 thick] 80 45 -ns-
1/2H [<0.50 thick] 57 25 7%
Regards, Wil Taylor