May 8, 2017 #1 uglyspec Mechanical Joined Dec 31, 2013 Messages 41 Location US Hello, If I have a shell and tube heat exchanger that has a non-welded (TEMA Type BEU) 2205 Duplex tubesheet, is impact testing required if the tubesheets is 1 1/2" thk? Thanks!
Hello, If I have a shell and tube heat exchanger that has a non-welded (TEMA Type BEU) 2205 Duplex tubesheet, is impact testing required if the tubesheets is 1 1/2" thk? Thanks!
May 8, 2017 #2 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,863 Location US Most likely, see UHA-51(d)(3)(a). What is the MDMT? Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand Upvote 0 Downvote
Most likely, see UHA-51(d)(3)(a). What is the MDMT? Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand
May 8, 2017 Thread starter #3 uglyspec Mechanical Joined Dec 31, 2013 Messages 41 Location US -20f Upvote 0 Downvote
May 9, 2017 #4 SJones Petroleum Joined Apr 22, 2001 Messages 3,945 Location GB http://www.eng-tips.com/viewthread.cfm?qid=422293 Steve Jones Corrosion Management Consultant http://www.linkedin.com/pub/8/83b/b04 All answers are personal opinions only and are in no way connected with any employer. Upvote 0 Downvote
http://www.eng-tips.com/viewthread.cfm?qid=422293 Steve Jones Corrosion Management Consultant http://www.linkedin.com/pub/8/83b/b04 All answers are personal opinions only and are in no way connected with any employer.
May 9, 2017 #5 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,863 Location US -20 F & over 3/8" thk, you are impact testing. Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand Upvote 0 Downvote
-20 F & over 3/8" thk, you are impact testing. Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand