I have a part (a spar/avaition part) that was suppose to be made from 2024-T3 alclad, instead it was made from 2024-T3 bare.
The finish spec call outs that the part can be anodic coated per Mil-a-8625 or Alodined per Mil-c-5541 (then one coat of primer). Pervouis batches (proper material) of parts have been alodined.
We want to keep the parts (cost and lead times on them are high) and the best choice would be to Chromic anodize/seal them.
I need some kind of justification/base though. So my question is if anybody knows of a document that compares the corrosion resistance of 2024 bare vs 2024 alclad for anodizing vs alodine?
The finish spec call outs that the part can be anodic coated per Mil-a-8625 or Alodined per Mil-c-5541 (then one coat of primer). Pervouis batches (proper material) of parts have been alodined.
We want to keep the parts (cost and lead times on them are high) and the best choice would be to Chromic anodize/seal them.
I need some kind of justification/base though. So my question is if anybody knows of a document that compares the corrosion resistance of 2024 bare vs 2024 alclad for anodizing vs alodine?