1965 18J6 Steel Joist Capacity 1

Status
Not open for further replies.

thinkhard

Structural
Sep 21, 2005
2
I'm working on a building constructed in 1965 that has 18J6 steel joists spanning 27 feet. Does anyone have a table from that time-frame that indicates what the capacity of the joist is?
 
Replies continue below

Recommended for you

Thanks SlideRuleEra. I actually have already ordered it but it hasn't arrived yet and I was hoping to keep moving forward if someone will help me out.
 
From ASD 7th:

Total allowable uniform=268 lb/ft and Fy=22 ksi

 