Is anyone aware of the reasons why the 1949 ASME Code dropped the stress allowables?
1943 and 1952 had an allowable stress of 13,750 for SA-285 C for example but in 1949 the allowable was dropped to 11,000.
1943 and 1952 had an allowable stress of 13,750 for SA-285 C for example but in 1949 the allowable was dropped to 11,000.