I am making a very simple flat spring clip to hold in a heater. When installed it is just slightly bent. The material I would like to use is 17-7PH full hard. Can I use this material in the full hard condition without further heat treatment? The temperature of the heater will go up to approx. 400-450C but only a small portion of the clip will be in contact. I used 1095 blue spring steel for the prototype but I am concerned about corrosion with time.