Tania Matsuo
Petroleum
Hi, I would like to know some literature about 17-7 alloy. We have a 17-7 HP spring that failed due to cracks. I am not sure if the heat treatment done was correct because I can visualize the inclusions using optical microscope (x100). The composition inclusion is Al end Fe and their shape are angulars. I am not sure if these kind of precipitation is regular.