this material can have so many heat treat conditions. H900, H1025, H1100........
i have one very small part, H-1025. i checked HRc, it reaches 44, higher than AMS spec. but as you know HRc is just for reference, not a base for rejection. (tensile listed as minimum)
what other metallurgical way to nail down the heat treat condition, as H-1025 relative lager elongation is critical to my application.
thanks.
i have one very small part, H-1025. i checked HRc, it reaches 44, higher than AMS spec. but as you know HRc is just for reference, not a base for rejection. (tensile listed as minimum)
what other metallurgical way to nail down the heat treat condition, as H-1025 relative lager elongation is critical to my application.
thanks.