We had a 15+" diameter bar of condition A, ASTM A705, 17-4 PH double aged to condition H1150. The hardness came out around 37 HRC. NACE requires the hardness to be 33 HRC max.
1. Any ideas as to what went wrong?
2. Would there be any bebefit to repeating the double aging process?
1. Any ideas as to what went wrong?