MaxCarb
Mechanical
- May 1, 2008
- 16
I'm selecting a material for a pump (impeller and shaft) in Sour Service as per NACE MR 0175.
My first choice is 17-4 PH above all becouse in the first period the service is not sour and for the future 200 ppm is indicated (very low).
My doubt is, with reference of section A.8 (Precipitation hardened stainless steels), which is the table to be taken in consideration for a pump? This also for other more corrosive cases.
Thanks in advance
My first choice is 17-4 PH above all becouse in the first period the service is not sour and for the future 200 ppm is indicated (very low).
My doubt is, with reference of section A.8 (Precipitation hardened stainless steels), which is the table to be taken in consideration for a pump? This also for other more corrosive cases.
Thanks in advance