15-5 is easily passivated and as posted above there is probably something amiss in the procedure. either in pickling or passivisation.
If you are pickling it the time, temperature, and concentration could wrong. The passivisation step is also open to problems especially if your pickling step is excessive. As in pickling, time, temperature, and concentration are important.
Awaiting your response.