Has anyone got cutting data that is faster than 114" or 2900mm a minute? for 12g Cr4, 5" or 7.5" lens. I am using 2kw laser but data for 1500w is equally useful.

Thanks in advance for any help.
 
Roy try this

(0.105 CRS STP F190)
( 5.0INCH NOZZLE=0.05IN NF-.04)
G88P5M56
M20
G87P30
M32
G82P1800Q100R20
G87P5
M22
G04X0.7
G88P30M56
G82P1300Q100R100F190
G87P0
M99
 
J Burgess

Thanks for the data, is q expressed as a percentage, ie is Q100 = 100%

 
Roy,

P is power
Q is frequency
R is duty cycle in %
F is feed rate