Jan 13, 2015 #1 Penguineer Mechanical Joined May 31, 2012 Messages 21 Location US Hello All - I have been searching for the endurance limit of 1045 cold-drawn steel bar but have thus far been unsuccessful. Does anyone know where I can search or have a source I could reference to get this value? Thank you.
Hello All - I have been searching for the endurance limit of 1045 cold-drawn steel bar but have thus far been unsuccessful. Does anyone know where I can search or have a source I could reference to get this value? Thank you.
Jan 13, 2015 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US I think your best bet will be to use the typical approximation of 1/2 UTS as high cycle fatigue strength. Good Luck otherwise. Upvote 0 Downvote
I think your best bet will be to use the typical approximation of 1/2 UTS as high cycle fatigue strength. Good Luck otherwise.