Hi everyone,
I am working on a weld procedure to weld A-516 Gr70 (P1 G2 ASTM material) to a forged 1030/1035 tube. 1030 and 1035 are not classified, so my procedure must use 1030 or 1035 to qualify it. My problem is I have been unable to find any 1030 or 1035 tube that is large enough. We need a 1-1/2" wall thickness to qualify use for the welded thickness on the end product.
This procedure will also be ABS approved, so it needs to be done on tube/pipe rather than plate. We disagree with this due to the size tube we are welding (28" OD), but would rather qualify with a tube rather than arguing with ABS for weeks over whether or not a plate will qualify a tube that large...
Do any of you have any idea where I can find 1030 or 1035 tube in the 1-1/2" wall range and at least 12" OD?
Thanks!
David Cox
I am working on a weld procedure to weld A-516 Gr70 (P1 G2 ASTM material) to a forged 1030/1035 tube. 1030 and 1035 are not classified, so my procedure must use 1030 or 1035 to qualify it. My problem is I have been unable to find any 1030 or 1035 tube that is large enough. We need a 1-1/2" wall thickness to qualify use for the welded thickness on the end product.
This procedure will also be ABS approved, so it needs to be done on tube/pipe rather than plate. We disagree with this due to the size tube we are welding (28" OD), but would rather qualify with a tube rather than arguing with ABS for weeks over whether or not a plate will qualify a tube that large...
Do any of you have any idea where I can find 1030 or 1035 tube in the 1-1/2" wall range and at least 12" OD?
Thanks!