Does anyone have a good starting parameters? I have my finger poised over the Like Button.

"I am stuck on Band-Aid brand, 'cause they are stuck on me"
 
Nevermid, we used same parameters as stainless and it seemed to work fine.

"I am stuck on Band-Aid brand, 'cause they are stuck on me"
 
close thread, nothing to see here